Yesterday I was able to complete the milling of the wax version of the medallion front. It's SMOOTH!! I changed the scale slightly from the file I gave to Michael, but it's still within spec for the rest of the design. We're going to cast this soon.







2 comments:

Have Blue said...

WOW, phenomenally smoother than the FDM prints! What cutter(s) did you use for the wax?

Frankie Flood said...

It was a .046875 4FL flat endmill. The step over was 5% of the endmill width though. It took a while but it was worth it.